Most mig welds form a glass line along one edge of the weld due to the flux. This needs to be removed by the fabricator. It cannot be removed by the normal galvanizing cleaning process and often is impossible to see during the process. This needs to be removed and repaired and is the fabricators responsibility.

glass, black, scale, lump